Laser 03 – Cutting parameters explained
Laser category. What each main setting in a CypCut cutting parameter does and what happens when it's wrong. Use it to read a parameter, not to change one: changes need manager approval (Laser 04). [REVIEW: general fibre-laser practice, check against our library]
Laser category. What each main setting in a CypCut cutting parameter does and what happens when it's wrong. Use it to read a parameter, not to change one: changes need manager approval (Laser 04). [REVIEW: general fibre-laser practice, check against our library]
1
Step 1 of 9

Each saved parameter is set for one material, thickness and gas. Load the right one (Laser 05). Don't change it without manager approval (Laser 04).

2
Step 2 of 9
<p>Power (W): more power cuts thicker or faster. Too low and it won&#39;t cut through. Too high and you get a wide kerf and burnt edges.</p>

Power (W): more power cuts thicker or faster. Too low and it won't cut through. Too high and you get a wide kerf and burnt edges.

3
Step 3 of 9
<p>Speed (mm/min): too fast and it won&#39;t cut through, with sparks flaring back up. Too slow and you get heavy dross and a rough, burnt edge.</p>

Speed (mm/min): too fast and it won't cut through, with sparks flaring back up. Too slow and you get heavy dross and a rough, burnt edge.

4
Step 4 of 9
<p>Gas and pressure: oxygen burns through mild steel and leaves an oxide edge. Nitrogen gives a clean, bright edge on stainless and aluminium. Air is a cheaper option for thin sheet. Low pressure leaves dross; too high on oxygen gives a rough cut.</p>

Gas and pressure: oxygen burns through mild steel and leaves an oxide edge. Nitrogen gives a clean, bright edge on stainless and aluminium. Air is a cheaper option for thin sheet. Low pressure leaves dross; too high on oxygen gives a rough cut.

5
Step 5 of 9
<p>Focus position (mm): where the beam focuses relative to the sheet. Wrong focus gives a wide kerf, dross or a failed cut. It&#39;s set in the parameter, for example 14.5 mm on 20 mm carbon steel O2 (Laser 14).</p>

Focus position (mm): where the beam focuses relative to the sheet. Wrong focus gives a wide kerf, dross or a failed cut. It's set in the parameter, for example 14.5 mm on 20 mm carbon steel O2 (Laser 14).

6
Step 6 of 9
<p>Nozzle and cut height: the nozzle type and size are listed at the top of the parameter (Laser 12). Cut height is the gap between the nozzle and the sheet, usually 0.5–1.5 mm. Too high and the cut gets wider and dirty.</p>

Nozzle and cut height: the nozzle type and size are listed at the top of the parameter (Laser 12). Cut height is the gap between the nozzle and the sheet, usually 0.5–1.5 mm. Too high and the cut gets wider and dirty.

7
Step 7 of 9
<p>Duty cycle and frequency: these are used for pulsed cutting on small holes and fine detail. Leave them as saved.</p>

Duty cycle and frequency: these are used for pulsed cutting on small holes and fine detail. Leave them as saved.

8
Step 8 of 9
<p>Pierce settings are separate from the cut settings. See Laser 06.</p>

Pierce settings are separate from the cut settings. See Laser 06.

9
Step 9 of 9
<p>If the cut is bad, check the nozzle, lens and centring first (Laser 12, 13, 15, 24) before you blame the parameter.</p>

If the cut is bad, check the nozzle, lens and centring first (Laser 12, 13, 15, 24) before you blame the parameter.