Before every cut the laser pierces a hole through the sheet. On thin sheet this takes a split second. On thick sheet it takes several stages.

3-stage pierce: on thick plate the head starts high with low power, then steps closer with more power, then drops to cutting height. This keeps spatter off the nozzle and lens.
The number of stages, plus the height, power, gas and stay time for each stage, are already saved in each cutting parameter. You don't set them by hand.

Stay time is how long the beam stays on at each stage before moving on. Our screen example is 100 ms.
Don't change pierce settings without manager approval.

If a pierce keeps failing, increase the stay time by 100 ms at a time until it pierces through.

A failed pierce blows spatter back at the nozzle. Check the nozzle afterwards and change it if it's damaged (Laser 12).